Note: According to different corrosion warranties, only the regional mandatory joining methods are allowed.
High Strength Low Alloy Steel
This information provides repair recommendations and general guidelines for
steel classified as High Strength Low Alloy Steel, also known
as HSLA. This type of steel normally has a tensile strength range from 300-700
MPa.
General Motors recommends the following when repairing or replacing th ...
Installation Procedure
Cut the front compartment front rail in corresponding locations to fit
the remaining original panel. The sectioning joint should be
trimmed to allow a gap of one-and-one-half-times the metal thickness at the
sectioning joint.
Create a 50 mm (2 in) backing plate from the unused porti ...
Air Hose Test
Caution: The air hose test should only be used on fully cured
urethane adhesive. Otherwise, damage to the urethane adhesive bead
could result in additional leaks.
Using a liquid detergent, diluted with water in a spray bottle, spray
the window at the edges. Begin at the bottom and grad ...